Table 4
Optical quality results of the seven laminated modules tested at 170 °C.
170 °C Set Temperature | 6 minutes process | 5 minutes process | |||||
---|---|---|---|---|---|---|---|
Category Recipe No. | #1 | #2 | #3 | #4 | #5 | #6 | #7 |
Backsheet optic | 1 | 5 | 1 | 8 | 5 | 10 | 10 |
Bubbles between cells | 10 | 10 | 10 | 10 | 10 | 10 | 10 |
Bubbles between strings | 10 | 10 | 10 | 10 | 10 | 10 | 10 |
Bubbles at the interconnection area | 10 | 10 | 10 | 10 | 10 | 10 | 10 |
String movement | 10 | 10 | 10 | 10 | 10 | 10 | 10 |
Backsheet shrinkage | 10 | 10 | 10 | 10 | 10 | 10 | 10 |
Cell breakage | 10 | 10 | 10 | 10 | 10 | 10 | 10 |