Open Access

Fig. 4

thumbnail

Download original image

(a) Evolution of film thickness (empty marks) and porosity (full symbols) of nanoporous structure deposited on FTO glass (squares) and ZnO:Al (triangles) with charge density consumed. (b) Evolution of the roughness factor of nanoporous films deposited on FTO glass (filled squares) on ZnO:Al (empty triangles) with the film thickness.